MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

PoolKemie SILIMOLD ADT-05 RTV2 silicon moulding rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Introduction: It is a two component room temperature vulcanizing pourable fluid silicon which cures on the addition of the appropriate CATALYST AD, according to the polyaddition process. SILIMOLD ADT 05 silicon rubber is characterized by its low hardness and no linear shrinkage.

Application: SILIMOLD ADT 05 silicon rubber is especially designed for heel inserts and inserts.

Peculiarities: Addition cure; Easy pour able; Faithfulness in details reproduction; Extreme mould release/mould life

Note 1: Tests have been carried out under these conditions: Temperature: +20°C; After: 24 ore; R.H.: 60%; Catalysis: 1:1

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1000 cP1000 cPComp. A, Before Catalysis, see note 1
 1000 cP1000 cPComp. B, Before Catalysis, see note 1
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inafter 5 days ageing, After Catalysis; ISO 4823
Storage Temperature 10.0 - 28.0 °C50.0 - 82.4 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8.08.0After Catalysis; DIN 53505
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourDemoulding time, See note 1, During Catalysis
Pot Life 15.0 min15.0 minSee note 1, During Catalysis
Shelf Life 12.0 Month12.0 MonthBoth components (A and B) in their original tightly closed containers, in a dry and cool place , away from moisture
 
Descriptive Properties
AppearanceFlexible rubberAfter Catalysis
 Thick LiquidBefore Catalysis
ColorTransparentComponent A, Before Catalysis
 TransparentComponent B, Before Catalysis
 TransparentAfter Catalysis
Mixing ratio1:1by weight, Before Catalysis

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOOLK012 / 318491

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.