MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Entec Ezprene® 9585A SHF TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: 85 Shore A TPE (Thermoplastic Vulcanizate). Available in black, natural for injection molding applications with long flow lengths or requires highly cosmetic surface. This soft, easy to color material is non-hydroscopic and offers excellent chemical resistance and physical properties. EZPrene is polyolefin based and is 100% recyclable.

Availability: North America

Features: Chemical Resistant; Fatigue Resistant; Good Adhesion; Good Colorability; Low to No Water Absorption; Ozone Resistant; Recyclable Material; Soft; UV Resistant

Appearance: Black; Natural Color

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.942 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84
@Time 5.00 sec
Extruded; ASTM D2240
 88
@Time 5.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 754 psiASTM D412
Tensile Stress 247 psi
@Strain 100 %
ASTM D412
Elongation at Break 490 %ASTM D412
Tear Strength 65.7 pliASTM D624
Compression Set 45 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 72 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -85.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 330 - 350 °FHopper, Extrusion
Rear Barrel Temperature 375 - 400 °F
Middle Barrel Temperature 385 - 410 °F
Front Barrel Temperature 385 - 410 °F
Nozzle Temperature 410 - 430 °F
Zone 1 340 - 375 °F
Zone 2 340 - 375 °F
Zone 3 340 - 375 °F
Zone 4 340 - 375 °F
Zone 5 340 - 375 °F
Adapter Temperature 375 - 410 °F
Die Temperature 375 - 410 °F
Melt Temperature 375 - 390 °FExtrusion
 390 - 430 °FInjection
Mold Temperature 75.0 - 125 °FInjection
Drying Temperature 180 °F
Dry Time 2.00 - 3.00 hour
Injection Pressure 750 - 1300 psi
Cushion 0.200 - 0.500 in
Screw Speed 30 - 80 rpmExtrusion
 50 - 200 rpmInjection
 
Descriptive Properties
Dynamic Service Temperature266°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB685 / 311378

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.