MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PolyMirae Moplen HF461Y Fiber (Melt-blown) Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: Addiform Moplen HF461Y is newly developed homopolymer particularly suitable for ultra fine denier melt-blown non-woven. It has ultra high melt flow and narrow molecular weight distribution which promotes thread line continuity and reduces fly or lint. Addiform Moplen HF461Y allows spinning of ultra fine denier fibers as well as high production speed with relatively low processing temperature. Moplen HF461Y resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.

Features: Excellent spinnability; Excellent drawability; Fine Denier; Higher productivity; Considerable energy saving (reduced processing temperature); Narrow molecular weight distribution; Anti-gas Fading

Applications: Diaper and Sanitary Napkin with Spunbond; Oil Absorbent Mat; Wipers; Air Filtration Media; Masks; Water Tissues; Base resin for color master batch

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 1500 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem CP1200B Homopolymer Polypropylene
Braskem H 152 Fiber Extrusion Polypropylene
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Braskem CP350WV Homopolymer Polypropylene
Braskem CP 741 Extrusion Polypropylene Heterophasic Copolymer

PMIRAE26 / 53138

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.