MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ FARADEX™ Compound DS0036I Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP FARADEX DS0036I compound is based on Polycarbonate (PC) resin containing 15% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding, High Impact, Non-Brominated & Non-Chlorinated Flame Retardant.

Features: EMI/RFI Shielding,Flame Retardant,Non-Chlorinated,Non-Brominated,High Impact Resistance,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ISO 1183
Water Absorption 0.13 %
@Time 86400 sec
0.13 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psi5 mm/min; ASTM D638
 55.0 MPa7980 psi5 mm/min; ISO 527
Tensile Strength, Yield 57.0 MPa8270 psi5 mm/min; ISO 527
 59.0 MPa8560 psi5 mm/min; ASTM D638
Elongation at Break 5.1 %5.1 %5 mm/min; ASTM D638
 4.0 - 8.0 %4.0 - 8.0 %5 mm/min; ISO 527
Elongation at Yield 3.8 %3.8 %5 mm/min; ISO 527
 4.3 %4.3 %5 mm/min; ASTM D638
Tensile Modulus 2.55 GPa370 ksi5 mm/min; ASTM D638
 2.80 GPa406 ksi1 mm/min; ISO 527
Flexural Strength 80.0 MPa11600 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.60 GPa377 ksi2 mm/min; ISO 178
Izod Impact Notched 124 J91.5 ft-lbASTM D256
 80.0 J
@Temperature -40.0 °C
59.0 ft-lb
@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 17.9 J/cm33.5 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²40.4 ft-lb/in²80*10*4; ISO 180/1U
Impact Test 29.0 J21.4 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 - 1.00e+6 ohm-cm10000 - 1.00e+6 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
Static Decay <= 0.010 sec<= 0.010 sec5000V to <50V; FTMS101B
Shielding Effectiveness 40 - 55 dB
@Thickness 3.00 mm
40 - 55 dB
@Thickness 0.118 in
SABIC method
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 57.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
31.7 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 68.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
37.8 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 110 °C230 °FUL 746B
UL RTI, Mechanical without Impact 115 °C239 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.60 mm
V-1
@Thickness >=0.0630 in
UL 94
 V-0
@Thickness >=2.00 mm
V-0
@Thickness >=0.0787 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 320 °C590 - 608 °F
Zone 3 320 - 330 °C608 - 626 °F
Melt Temperature 305 - 325 °C581 - 617 °FInjection Molding
Mold Temperature 95.0 - 120 °C203 - 248 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80628 / 288575

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.