MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC™ EX39F ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Viscosity 1.52e+6 cP
@Shear Rate 100 1/s,
Temperature 240 °C
melt; ASTM D3825
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 28.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 35.0 MPa5 mm/min; ASTM D638
Elongation at Break 108 %5 mm/min; ASTM D638
Elongation at Yield 3.5 %5 mm/min; ASTM D638
Tensile Modulus 1680 MPa5 mm/min; ASTM D638
Flexural Yield Strength 57.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1900 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 464 J/mASTM D256
 320 J/m
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 39.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 101 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 117 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 106 °CRate B/50; ASTM D1525
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.52 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 1 195 - 210 °CSheet Extrusion
Zone 2 200 - 220 °CSheet Extrusion
Zone 3 205 - 230 °CSheet Extrusion
Zone 4 210 - 235 °CSheet Extrusion
Adapter Temperature 200 - 225 °CSheet Extrusion
Die Temperature 210 - 240 °CSheet Extrusion
Melt Temperature 210 - 240 °C
Drying Temperature 90.0 - 95.0 °CSheet Extrusion
Dry Time 2.00 - 4.00 hourSheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10017 / 243484

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.