MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound GL003 Polysulfone (PSU) (Asia)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: LNP LUBRICOMP GL003 compound is based on Polysulfone (PSU) resin containing 15% PTFE. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccASTM D792
 1.31 g/ccISO 1183
Moisture Absorption 0.0500 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0076 cm/cm24hrs; ISO 294
 0.0076 cm/cmSABIC method
 0.0070 - 0.0090 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm24hrs; ASTM D955
 0.0083 cm/cm24hrs; ISO 294
 0.0083 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPaASTM D638
 55.0 MPa5 mm/min; ASTM D638
 55.0 MPaISO 527
 55.0 MPa5 mm/min; ISO 527
Elongation at Break 9.9 %ASTM D638
 10 %5 mm/min; ASTM D638
 11.8 %ISO 527
 11.8 %5 mm/min; ISO 527
Flexural Strength 75.0 MPaASTM D790
 78.0 MPaISO 178
 78.0 MPayield, 2 mm/min; ISO 178
 82.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2060 MPaASTM D790
 2070 MPa1.3 mm/min, 50 mm span; ASTM D790
 2300 MPaISO 178
 2300 MPa2 mm/min; ISO 178
Izod Impact Notched 58.0 JASTM D256
Izod Impact, Unnotched 891 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.23ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.12ASTM D3702 Modified: Manual
K (wear) Factor 24.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 179 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 178 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 175 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 170 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 340 - 350 °C
Zone 3 350 - 360 °C
Melt Temperature 360 - 370 °CInjection Molding
Mold Temperature 150 °C
Drying Temperature 120 - 150 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80790 / 288737

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.