MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin PX1860 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL PX1860 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR additives to achieve a V1 UL94 rating at 1.5 mm with a specific density of 1.1 g/cm^3. NORYL PX1860 may be an excellent material candidate for Flat Panel TV enclosure applications requiring good rheological properties, heat resistance, hydrolysis resistance, low density and thin wall flame resistance.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Density 1.10 g/ccISO 1183
Moisture Absorption 0.0200 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.13 %ISO 62-1
Viscosity 15 cP
@Load 1.20 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 34 cP
@Load 2.16 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 49.0 MPa50 mm/min; ASTM D638
 53.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 52.0 MPa50 mm/min; ASTM D638
 61.0 MPa50 mm/min; ISO 527
Elongation at Break 7.3 %50 mm/min; ASTM D638
 8.0 %50 mm/min; ISO 527
Elongation at Yield 3.5 %50 mm/min; ISO 527
 3.6 %50 mm/min; ASTM D638
Tensile Modulus 2510 MPa1 mm/min; ISO 527
 3140 MPa50 mm/min; ASTM D638
Flexural Strength 89.0 MPayield, 2 mm/min; ISO 178
 98.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2420 MPa2 mm/min; ISO 178
 2770 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 38.0 JASTM D256
 27.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 4.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 6.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cmASTM D257
 4.00e+16 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmASTM D257
 1.00e+14 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
ASTM D150
 2.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 28.6 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
 0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 - 250 VUL 746A
 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 110 °CRate B/50; ASTM D1525
 111 °CRate B/50; ISO 306
 114 °CRate B/120; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
Oxygen Index 30 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 250 - 280 °C
Zone 2 240 - 270 °C
Zone 3 260 - 295 °C
Melt Temperature 260 - 295 °CInjection Molding
Mold Temperature 45.0 - 70.0 °C
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 65.0 - 85.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82448 / 290395

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.