MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC CYCOLOY™ FR CE3510 PC+ABS (Europe)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CE3510 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is a high impact, non chlorinated/brominated flame retardant grade that can be injection molded or extruded. It has an MVR (260°C/5kg) of 8 and a UL94 V0@1.5mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inSABIC method
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 500 °F
cm³/10 min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 49.0 MPa7110 psi50 mm/min; ASTM D638
 50.0 MPa7250 psi50 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa9280 psi50 mm/min; ASTM D638
 65.0 MPa9430 psi50 mm/min; ISO 527
Elongation at Break 35 %35 %50 mm/min; ASTM D638
 >= 50 %>= 50 %50mm/min; ISO 527
Elongation at Yield 4.3 %4.3 %50 mm/min; ASTM D638
 4.6 %4.6 %50 mm/min; ISO 527
Tensile Modulus 2.68 GPa389 ksi50 mm/min; ASTM D638
Flexural Yield Strength 95.0 MPa13800 psi1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPa13800 psi2 mm/min; ISO 178
Flexural Modulus 2.47 GPa358 ksi2 mm/min; ISO 178
 2.61 GPa379 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.64 J/cm12.4 ft-lb/inASTM D256
 1.09 J/cm
@Temperature -30.0 °C
2.04 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²80*10*4; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
 14.0 kJ/m²
@Temperature 0.000 °C
6.66 ft-lb/in²
@Temperature 32.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.40 J/cm²
@Temperature -30.0 °C
6.66 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  18.0 kV/mm
@Thickness 3.20 mm
457 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 27.0 kV/mm
@Thickness 1.60 mm
686 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 44.0 kV/mm
@Thickness 0.800 mm
1120 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 75.0 °C167 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 111 °C232 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 111 °C
@Thickness 3.20 mm
232 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 100 °C212 °F1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 100 °C
@Thickness 3.20 mm
212 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 116 °C241 °FRate B/50; ISO 306
 118 °C244 °FRate B/120; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
Glow Wire Test  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
1520 °F
@Thickness 0.118 in
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature
 60.0 - 80.0 °C140 - 176 °FHopper Temperature
Nozzle Temperature 250 - 280 °C482 - 536 °FInjection Molding
Zone 1 235 - 260 °C455 - 500 °FProfile Extrusion
 240 - 270 °C464 - 518 °F
Zone 2 240 - 265 °C464 - 509 °FProfile Extrusion
 245 - 275 °C473 - 527 °F
Zone 3 245 - 270 °C473 - 518 °FProfile Extrusion
 250 - 280 °C482 - 536 °F
Zone 4 245 - 270 °C473 - 518 °FProfile Extrusion
Adapter Temperature 245 - 270 °C473 - 518 °FProfile Extrusion
Die Temperature 235 - 260 °C455 - 500 °FProfile Extrusion
Melt Temperature 230 - 270 °C446 - 518 °F
 250 - 280 °C482 - 536 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °FProfile Extrusion
 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourProfile Extrusion
 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %0.020 %
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FCalibrator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10788 / 244255

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.