MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Caplinq LINQSTAT™ VCF Low-Level Surface Conductive Polyethylene Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE)

Material Notes: CAPLINQLINQSTAT™ VCF-Series is a black, carbon-filled, electrically conductive polyethylene plastic film designed to provide both physical and static protection. Having a surface resistance of <200,000ohm/sq, (2x105O/sq) it offers medium-level static protection which means it effectively avoids accumulation of electric charge on itself and the products which it protects. Its easy-grounding nature makes it ideal for packaging where electrostatic contamination is a problem. CAPLINQ LINQSTAT™ VCF-Series is useful in applications where the key is to balance cost versus performance. As a medium-level surface conductive plastic, the carbon-loading is such that it is low-enough to be cost-effective, while being high enough to meet the electrical requirements of military specification MIL-PRF-81705D Type II and MIL-P-82646A. CAPLINQ LINQSTAT™VCF-Series film and its conductivity are unaffected by humidity and age. The film is heat-sealable, flexible and offers exceptional abrasion resistance. The film gives good thermal stability and has outstanding chemical resistance. It has a standard thickness range from 50.8µm to 200µm (0.002” to 0.008”) and is available in sheeting, tubing and bag versions. Roll lengths and widths vary depending on thickness and application.

Applications:

  • Protection and storage of static-sensitive components
  • Interleaver between layers of smart cardchips
  • Grounding Mats
Product Features & Benefits:
  • Surface conductive plastic
  • Black Opaque –Printable
  • Provides Anti-Static protection to electronics components
  • Groundable
  • Humidity independent conductivity
  • Meets military specification MIL-P-82646A
Chemical Susceptibility:
  • Methanol: Resistant
  • Ethanol: Resistant
  • Isopropanol: Resistant
  • Weak Acids: Resistant
  • Ketones (Acetone): Slow Attack
  • Weak Alkalines: Slow Attack
  • Hydrocarbons: Non-Resistant

Information provided by Caplinq

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 13.8 MPaASTM-D882
Film Elongation at Break, MD 330 %ASTM-D882
Film Elongation at Break, TD 390 %ASTM-D882
Dart Drop Test 380 - 400 g50% Failure Weight; ASTM D1709-67 Method B
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 200000 ohmMIL-PRF-81705D Type II
Static Decay <= 2.0 secEIA-Std541
 
Descriptive Properties
Heat Seal Strength (% of Tensile Strength)0.82Transverse Direction, ASTM-D882
 0.96Machine Direction, ASTM-D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCAPL1017 / 256017

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.