MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akrochem RETARDER SAFE
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: A non-staining and non-discoloring retarder for natural and synthetic rubber compounds. Use from 0.10 to 2.0 parts per 100 rhc, depending on polymer and accelerator system used. Very effective with thiazoles, sulfenamides, and dithiocarbamates. Not effective in low sulfur thiuram cures. Also useful for replasticizing of slightly scorched stocks by cold mill mixing. Does not bloom at recommended amounts and no odor occurs from the use of Retarder SAFE. Does not significantly change the fully cured characteristics of the compound.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.68 g/cc1.68 g/cc
Particle Mesh Size 100 Mesh100 Mesh1.0% maximum retained
 
Thermal PropertiesMetricEnglishComments
Melting Point 108 - 113 °C226 - 235 °F
 
Descriptive Properties
AppearanceWhite to Tan Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH578 / 315496

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.