MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Europrene® SSBR K SOL R C 2525 Solution-Styrene Butadiene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Solution polymerized styrene-butadiene rubber is obtained by the anionic polymerization of styrene and butadiene initiated by lithium alkyls in hydrocarbon solvent, the distribution of styrene units in the polymer chain results in either block or random co-polymers. Block S-SBRs have a lower styrene content than Random S-SBRs and are more suitable for calendaring and extrusion processes. They are also used for bitumen modification and for the production of adhesive and high impact polystyrene and ABS resins. Random S-SBRs provide a versatile support for tailor made product operation through the styrene content and microstructure of butadiene units allowing good performance in terms of process ability, rolling resistance, grip and abrasion and becoming the first preference in the tire sector.

Applications: Carbon black based compound for low rolling resistance treads, mechanical goods, footwear.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 54
@Temperature 100 °C
 
Chemical PropertiesOriginal ValueComments
Styrene Content 26 %bound. % wt
 
Descriptive Properties
Polymerization ProcessContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9974 / 265613

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.