System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Syensqo (Solvay Specialty Polymers) Hylar® 301S PVDF
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polyvinylidene Fluoride (PVDF)
;
Polyvinylidinefluoride (PVDF), Molded/Extruded
Material Notes:
Hylar® 301S is a high melt viscosity polyvinylidene fluoride (PVDF) powder used for non-architectural dispersion coatings.
Applications: Coating Applications
Features: High Viscosity; Homopolymer
Information provided by Solvay Specialty Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.75
-
1.77
g/cc
ASTM D1505
Water Absorption at Saturation
0.020 %
ASTM D570
Viscosity
2900
-
3300
cP
Melt; ASTM D3835
Thermal Properties
Original Value
Comments
Heat of Fusion
40.0
J/g
ASTM D3418
Specific Heat Capacity
1.30
J/g-°C
ASTM C351
Melting Point
160
°C
Crystallization Temperature
124
°C
Peak; ASTM D3418
Optical Properties
Original Value
Comments
Gloss
25 %
60°; ASTM D2457
Descriptive Properties
Availability
Europe
North America
Forms
Powder
Processing
Coating
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSOL8Y4255 / 280055
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.