MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ MB006S PP (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
 1.12 g/ccASTM D 792
Moisture Absorption 0.0200 %
@Time 86400 sec
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.0116 cm/cm
@Time 86400 sec
ISO 294
 0.012 cm/cm
@Time 86400 sec
ASTM D 955
Linear Mold Shrinkage, Transverse 0.011 cm/cm
@Time 86400 sec
ASTM D 955
 0.0115 cm/cm
@Time 86400 sec
ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 19.0 MPaASTM D 638
 19.0 MPaISO 527
Tensile Strength, Yield 24.0 MPaASTM D 638
 24.0 MPaISO 527
Elongation at Break 83.4 %ISO 527
 87.5 %ASTM D 638
Elongation at Yield 5.5 %ISO 527
 6.3 %ASTM D 638
Tensile Modulus 2400 MPa1 mm/min; ISO 527
Flexural Strength 44.0 MPaASTM D 790
 46.0 MPaISO 178
Flexural Modulus 2130 MPaASTM D 790
 2900 MPaISO 178
Izod Impact, Notched 21.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 234 J/m
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1U
Impact Test 1.00 JMultiaxial Impact; ISO 6603
Instrumented Impact Energy at Peak 3.00 J
@Temperature 23.0 °C
ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 68.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 112 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 70.0 °C
@Thickness 3.20 mm
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass
Overview of materials for Polypropylene with 20% Glass Fiber Filler
LATI Latimass 47/7-04 D008 PP Copolymer

PSABI47002 / 188087

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.