MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ GF008 PSU (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.

This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccASTM D 792
 1.60 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
@Time 86400 sec
ASTM D 955
 0.0010 - 0.0040 cm/cm
@Time 86400 sec
ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Time 86400 sec
ASTM D 955
 0.0030 - 0.0050 cm/cm
@Time 86400 sec
ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 108 MPaASTM D 638
 113 MPaISO 527
Elongation at Break 1.4 %ASTM D 638
 1.4 %ISO 527
Tensile Modulus 11650 MPa50 mm/min; ASTM D 638
Flexural Strength 158 MPaASTM D 790
 164 MPaISO 178
Flexural Modulus 9900 MPaISO 178
 11700 MPaASTM D 790
Izod Impact, Notched 64.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 3.79 J/cm
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1U
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 180 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 176 °C
@Thickness 3.20 mm
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® S 6010 PSU
BASF Ultrason® S 2010 PSU

PSABIC5292 / 119180

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.