MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Inov Chem Donfoam 603 ECOMATE Base blend polyols
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: "Wood Imitation" structure foam, is a new type of carving synthetic materials, Donfoam 603 use ECOMATE as blowing agent. It has high mechanical strength and hardness, simple molding process, high production efficiency and excellent appearance. Characteristics are as follows,
1. Excellent repetition molding property. It not only can mould certain shape size, but also mould lifelike wood texture and other designs, good touch
2. appearance and feel close to wood , which could be planed, nailed, drilled, and carved patterns or designs .
3. Mold can be aluminum or steel, and silicon rubber, epoxy resin or other resins, which are low cost and easy machining.
4. Process is simple, fast, high efficiency of qualified.
5. Physical and mechanical properties is one of optimal synthesis wood produced by various polymer. Physical property can be controlled by adjusting the formula.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 - 1.12 g/cc
Density 0.0600 - 0.300 g/ccFree density
 0.100 - 0.400 g/ccFoam Performances
Viscosity 800 - 1500 cP
Storage Temperature 10.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 35 - 70
Tensile Strength 5.00 MPa
Compressive Strength 5.00 - 7.00 MPa
 
Processing PropertiesOriginal ValueComments
Cure Time 200 - 220 secTack free time
Gel Time 2.33 - 2.67 min
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceLight yellow to brown yellow viscous liquid
Curving strength7-10 MPa
Hydroxyl value250-400 mgKOH/g
Recommended Ratio100DFM-103 polyols
 100-105Isocyanate
Rise time50-70 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINOVCHM026 / 312555

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.