MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound DX11355 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP DX11355 compound is based on Polycarbonate (PC) resin containing proprietary fillers and available in black color only. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Impact, Non-Brominated, Non-Chlorinated Flame Retardant.

Features: Enhanced Ductility,Laser Direct Structuring,Flame Retardant,Circuit Solution,Colorable,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccASTM D792
Moisture Absorption 0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm24hrs; ASTM D955
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 58.0 MPa50 mm/min; ASTM D638
Elongation at Break 70 %50 mm/min; ASTM D638
Elongation at Yield 5.4 %50 mm/min; ASTM D638
Tensile Modulus 2600 MPa50 mm/min; ASTM D638
Flexural Strength 89.0 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 90.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2400 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 800 JASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.92
@Frequency 1e+9 Hz
IEC 60250
Dissipation Factor 0.0070
@Frequency 1e+9 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 62.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 67.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.600 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °C
Zone 2 255 - 295 °C
Zone 3 260 - 300 °C
Melt Temperature 275 - 300 °CInjection Molding
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 100 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 40 - 70 rpm
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81562 / 289509

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.