MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bayport Polymers Baystar™ BM359SG HDPE, blow molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: BM359 SG has been especially designed for the manufacture of blow molded bottles (up to 5 liters) with a superior surface gloss and contact transparency. It is recommended either in mono-layer applications for flexible bottles (e.g. squeeze-able bottles) or in co-extrusion with BM593 for rigid bottles. Typical applications are, both in mono and in co-extrusion, differentiated bottles for personal care products and aggressive liquids (e.g. detergents,…).

BM359 SG, a metallocene resin, has a very specific molecular structure that yields superior optical properties as well as an excellent processability. It can be processed easily on conventional equipment both in mono and in co-extrusion. The use of BM359 SG along with BM593 (a bimodal HDPE, based on hexene as co-monomer) in co-extrusion offers an attractive mean to maximize the compromise between easy processability, stress crack resistance, bottle rigidity and superior surface gloss.

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.935 g/ccISO 1183
Environmental Stress Crack Resistance >= 1000 hour100% ant.; ASTM D1693-70
Melt Flow 0.90 g/10 min
@Load 2.16 kg
ISO 1133
High Load Melt Index 25 g/10 min
@Load 21.6 kg
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 35.0 MPaISO 527
Tensile Strength, Yield 17.0 MPaISO 527
Elongation at Break >= 700 %ISO 527
Elongation at Yield 12 %ISO 527
Flexural Modulus 0.650 GPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 °FASTM D3417
 
Optical PropertiesOriginal ValueComments
Gloss 60 - 90 %60 Degrees

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bayport Polymers Baystar™ Lumicene® mPE BM 359 SG Metallocene Medium Density High Gloss Blow Molding Resin

PBAYST813x / 38633

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.