MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Potassium chlorate
Categories: Other Engineering Material

Material Notes: Potassium chlorate (KClO3) is formed through electrolysis and crystallization, with final properties formed through grinding and sieving. Potassium chlorate is generally used in pyrotechnics and the match industry.

CAS number: 3811-04-9

Applications: With increasingly high demands on safety, efficiency and quality of the end products, producers of pyrotechnics are increasing their demands on raw materials and their suppliers. With its supreme quality product, high service level and advanced knowledge of Health/Safety/Environment, Nouryon has proven to be an invaluable partner to the pyrotechnical industry. Additionally we produce several grades of potassium chlorate that are tailor-made to meet the specific demands of match manufacturers in all parts of the world. This is the result of a long and close cooperation with manufacturers around the globe.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.20 - 1.40 g/cc
Density 2.34 g/cc
Molecular Weight 122.55 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 356 °C
Boiling Point 400 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY858 / 286381

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.