Aramid fiber reinforced PA66, heat stabilized, friction & wear modified. It can easily be processed on most injection molding machines. Tribocomp® PA66 AF15 TS0 is an aramid fiber reinforced PA66 that is heat stabilized and friction and wear modified. It can easily be processed on most injection molding machines. Information provided by Solvay Specialty Polymers. |