MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Poco Graphite Premium Graphite Thermal Management Graphite Material Pocofoam® Graphite Foam
Categories: Carbon; Graphite

Material Notes: Pocofoam® graphite foam is a low density, high porosity thermal management material ideally suited to handle intermittent temperature loads. Created through a partnership with Oakridge National Labs, Pocofoam® graphite foam was developed to create unidirectional heat. This grade has low density and high porosity to handle speed-of-heat transfer. Features: Highly controlled microstructure provides reliable product performance. Unilateral thermal conductivity funnels heat from sensitive electronics. Radiofrequency shielding reduces outside interference from readings. High purity maintains process integrity. Chemically inert material properties keep material from reacting to most acids or organic solvents.

Applications: Electronics. Aerospace Medical. Ultrasound. Transducers.

Information provided by Entegris POCO Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.500 g/cc0.0181 lb/in³
Open Porosity 96 %96 %
Porosity 75 %75 %Total
Pore Size 400 microns15.7 mil
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 2.76 MPa400 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  -0.700 µm/m-°C
@Temperature -233 - 127 °C
-0.389 µin/in-°F
@Temperature -387 - 261 °F
Out of plane
 0.000 - 0.800 µm/m-°C
@Temperature 300 - 1000 °C
0.000 - 0.444 µin/in-°F
@Temperature 572 - 1830 °F
Out of plane
 0.600 µm/m-°C
@Temperature -233 - 127 °C
0.333 µin/in-°F
@Temperature -387 - 261 °F
In plane
 1.30 - 2.00 µm/m-°C
@Temperature 300 - 1000 °C
0.722 - 1.11 µin/in-°F
@Temperature 572 - 1830 °F
In plane
Thermal Conductivity 45.0 W/m-K312 BTU-in/hr-ft²-°FIn plane
 135 W/m-K937 BTU-in/hr-ft²-°FOut of plane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CPOCO408 / 268793

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.