MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Armeen CD Primary amine
Categories: Other Engineering Material

Material Notes: Armeen CD is a distilled coco amine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.774 g/cc
@Temperature 70.0 °C
0.0280 lb/in³
@Temperature 158 °F
 0.781 g/cc
@Temperature 60.0 °C
0.0282 lb/in³
@Temperature 140 °F
 0.790 g/cc
@Temperature 38.0 °C
0.0285 lb/in³
@Temperature 100 °F
 0.805 g/cc
@Temperature 25.0 °C
0.0291 lb/in³
@Temperature 77.0 °F
Viscosity  33.6 cP
@Temperature 75.0 °C
33.6 cP
@Temperature 167 °F
 34.5 cP
@Temperature 65.0 °C
34.5 cP
@Temperature 149 °F
 37.8 cP
@Temperature 55.0 °C
37.8 cP
@Temperature 131 °F
 41.4 cP
@Temperature 45.0 °C
41.4 cP
@Temperature 113 °F
 44.2 cP
@Temperature 35.0 °C
44.2 cP
@Temperature 95.0 °F
Vapor Pressure 0.00130 bar0.975 torr
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.34 J/g-°C
@Temperature 25.0 - 30.0 °C
0.559 BTU/lb-°F
@Temperature 77.0 - 86.0 °F
 2.40 J/g-°C
@Temperature 42.2 - 45.0 °C
0.573 BTU/lb-°F
@Temperature 108 - 113 °F
 2.42 J/g-°C
@Temperature 48.9 - 51.1 °C
0.579 BTU/lb-°F
@Temperature 120 - 124 °F
Melting Point 18.0 °C64.4 °F
Boiling Point  2.00 °C
@Pressure 0.00466628 MPa
35.6 °F
@Pressure 0.676611 psi
 8.00 °C
@Pressure 0.00786602 MPa
46.4 °F
@Pressure 1.14057 psi
 32.0 °C
@Pressure 0.011599 MPa
89.6 °F
@Pressure 1.6819 psi
 180 °C
@Pressure 0.101325 MPa
356 °F
@Pressure 14.6921 psi
Pour Point 18.0 °C64.4 °F
Flash Point >= 150 °C>= 302 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 0.00 - 1.00.00 - 1.0
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number275-288 mg KOH/g
AppearanceLiquid
Cloud point19°C
Content= 2 %Secondary Amine
 = 98 %Primary Amine
 0-12 g I2/100 gIodine value
 195-204 g/eqNeutralization equivalent
Equivalent mass202 g/eq
HLB10.3Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY195 / 285718

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.