MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECATEC SAN NAF45 T300 CP/IP/OS V01 natural SAN, 45% Flax Fiber Reinforced
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes:
  • low density
Target Industries:
  • automotive industry
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³
Filler Content 45 %45 %Fiber volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 130 MPa18900 psiISO 527-4
Modulus of Elasticity 19.0 GPa2760 ksiISO 527-4
Flexural Strength 180 MPa26100 psiISO 14125
Flexural Modulus 16.0 GPa2320 ksiISO 14125
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C8.33 µin/in-°F
CTE, linear, Transverse to Flow 15.0 µm/m-°C8.33 µin/in-°F
Maximum Service Temperature, Air 90.0 °C194 °Flong term
 100 °C212 °Fshort term
Glass Transition Temp, Tg 110 °C230 °F
 
Processing PropertiesMetricEnglishComments
Drying Temperature 80.0 °C176 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour
 
Descriptive Properties
Colornatural
Fiber volume content (%)45
General material information0.46 mmply thickness (consolidated)
 1000 mmMaterial widths
 300 g/m²Fiber areal weight
 573 g/m²Areal weight finished product
 Flax fibersFiber type
 Twill 2/2Fiber architecture
Resin weight content (%)47.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8258 / 319186

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.