Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength | 39.3 MPa @Temperature 82.2 °C | 5700 psi @Temperature 180 °F |
| 40.0 MPa @Temperature -55.0 °C | 5800 psi @Temperature -67.0 °F |
| 42.1 MPa @Temperature 22.8 °C | 6100 psi @Temperature 73.0 °F |
| 1860 MPa @Temperature 82.2 °C | 270000 psi @Temperature 180 °F |
| 1970 MPa @Temperature 22.8 °C | 286000 psi @Temperature 73.0 °F |
| 1990 MPa @Temperature -55.0 °C | 289000 psi @Temperature -67.0 °F |
Tensile Modulus | 316.8 GPa @Temperature 22.8 °C | 45950 ksi @Temperature 73.0 °F |
| 319.8 GPa @Temperature 82.2 °C | 46390 ksi @Temperature 180 °F |
| 321.8 GPa @Temperature -55.0 °C | 46670 ksi @Temperature -67.0 °F |
Compressive Strength | 78.6 MPa @Temperature 82.2 °C | 11400 psi @Temperature 180 °F |
| 890.1 MPa @Temperature 22.8 °C | 129100 psi @Temperature 73.0 °F |
| 939.8 MPa @Temperature -55.0 °C | 136300 psi @Temperature -67.0 °F |
Compressive Modulus | 316.3 GPa @Temperature -55.0 °C | 45880 ksi @Temperature -67.0 °F |
| 331 GPa @Temperature 82.2 °C | 48000 ksi @Temperature 180 °F |
| 341.0 GPa @Temperature 22.8 °C | 49460 ksi @Temperature 73.0 °F |
Shear Modulus | 4.27 GPa | 620 ksi |
Shear Strength | 75.2 MPa | 10900 psi |
| 53.8 MPa @Temperature 82.2 °C | 7800 psi @Temperature 180 °F |
| 73.8 MPa @Temperature -4.44 °C | 10700 psi @Temperature 24.0 °F |
| 86.9 MPa @Temperature -55.0 °C | 12600 psi @Temperature -67.0 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Constant | 3.45 @Frequency 9.375e+6 Hz, Temperature 121 °C | 3.45 @Frequency 9.375e+6 Hz, Temperature 250 °F |
| 5.54 @Frequency 9.375e+6 Hz, Temperature 23.9 °C | 5.54 @Frequency 9.375e+6 Hz, Temperature 75.0 °F |
Dielectric Loss Index | 0.00800 @Frequency 9.375e+6 Hz, Temperature 23.9 °C | 0.00800 @Frequency 9.375e+6 Hz, Temperature 75.0 °F |
| 0.0120 @Frequency 9.375e+6 Hz, Temperature 121 °C | 0.0120 @Frequency 9.375e+6 Hz, Temperature 250 °F |
|
Thermal Properties | Metric | English | Comments |
---|
Glass Transition Temp, Tg | 160.4 °C @Temperature 82.2 °C | 320.7 °F @Temperature 180 °F |
| 169.6 °C @Temperature 23.9 °C | 337.3 °F @Temperature 75.0 °F |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding