MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Duratherm DuraClean Heat Exchanger System Cleaner
Categories: Fluid

Material Notes: DuraClean is a long life, preventative maintenance system cleaner. In addition to its ability to function as a long-term heat transfer fluid, DuraClean effectively dissolves sludge and carbon build-up in tanks and process piping without disrupting production. DuraClean is the perfect preventative maintenance tool. It’s capable of running in systems at temperatures up to 288°C (550°F) and it’s odorless. It easily handles long term operation while seamlessly allowing production to continue uninterrupted for a complete oil cycle. DuraClean is also available in Food Grade.

Information provided by Duratherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Kinematic Viscosity 44.6 cSt
@Temperature 104 °C
44.6 cSt
@Temperature 219 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 287 °C549 °FBulk/Use Temp.
Flash Point 240 °C464 °F
 
Descriptive Properties
ApplicationLight to moderately fouled systems
Flushing Required?No
Recommended Concentration (%)100
Run ProductionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDURA689 / 287882

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.