MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL EVA 6055 EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: MARPOL® EVA 6055 is a fractional melt index 6.5% EVA copolymer designed for films requiring excellent toughness and good heat sealing characteristics.

Recommended Applications: Frozen food packaging, fresh food packaging, ice bags, and heavy duty produce bags.

Additives: Antiblock – no, Slip – no.

Processing Notes: Melt temperatures of 360°F – 390°F (182 °C - 200 °C) are recommended for this resin. This resin grade complies with 21 CFR 177.1350.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.929 g/ccASTM D1505
Vinyl Acetate Content 6.5 %
Melt Flow 0.55 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 380 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Flexural Modulus, 1% Secant 15000 psiMD; ASTM D882
 16000 psiTD; ASTM D882
Elmendorf Tear Strength MD 150 gASTM D1922
Elmendorf Tear Strength, MD 250 g/milASTM D1922
Dart Drop Test 480 gASTM D1709
Film Tensile Strength at Break, MD 3500 psiUltimate; ASTM D882
Film Tensile Strength at Break, TD 3700 psiUltimate; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 102 °CPeak; ASTM D3418
Vicat Softening Point 81.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.8 %ASTM D1003
Gloss 74 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 200 °C
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO206 / 283803

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.