MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Hytrel® 6356BKB High Performance Polyester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes:

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
cm³/10min Volumetric; ISO 1133
 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 63ISO 48-4
Tensile Modulus 280 MPaISO 527-1/-2
Flexural Modulus 290 MPaISO 178
Poissons Ratio 0.48
Charpy Impact, Notched 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 120 kJ/m²
@Temperature 23.0 °C
Partial Break; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 210 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75-1/-2
Glass Transition Temp, Tg -5.00 °C10°C/min; ISO 11357-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 °COptimum, Extrusion
 225 - 240 °CRange, Extrusion
 240 °COptimum, Injection
 235 - 260 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 100 °CInjection
 90.0 - 110 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
Hold Pressure <= 70.0 MPaInjection
 
Descriptive Properties
Drying RecommendedyesInjection
PolymerTPC
Regional AvailabilityNorth America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4551 / 280497

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.