MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC LNP™ KONDUIT™ Compound OX11315 Polyphenylene Sulfide, Linear (PPS, Linear)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LNP KONDUIT OX11315 compound is based on Polyphenylene Sulfide (PPS) resin containing minerals. Added features of this grade include: Thermally Conductive, Electrically Insulative and Non-Brominated, Non-Chlorinated Flame Retardant.

Features: Electrically Isolative,Flame Retardant,Thermally Conductive,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Density 1.76 g/cc0.0636 lb/in³ASTM D792
Moisture Absorption 0.0100 %0.0100 %23°C/50% RH/24 hrs; ASTM D570
 0.0100 %0.0100 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0034 cm/cm0.0034 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0044 cm/cm0.0044 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.0 MPa5950 psi5 mm/min; ASTM D638
 54.0 MPa7830 psi5 mm/min; ISO 527
Elongation at Break 0.20 %0.20 %5 mm/min; ASTM D638
 0.30 %0.30 %5 mm/min; ISO 527
Tensile Modulus 18.38 GPa2666 ksi1 mm/min; ISO 527
 30.1 GPa4370 ksi5 mm/min; ASTM D638
Flexural Strength 82.0 MPa11900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 84.0 MPa12200 psiISO 178
Flexural Modulus 21.38 GPa3101 ksi2 mm/min; ISO 178
 26.5 GPa3840 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 16.0 J11.8 ft-lbASTM D256
Izod Impact, Unnotched 0.540 J/cm1.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 1.00 kJ/m²0.476 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 3.00 kJ/m²1.43 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 J3.69 ft-lbASTM D3763
Impact Test 1.00 J0.738 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 2.40e+15 ohm2.40e+15 ohmASTM D257
Dielectric Strength 1.20 kV/mm
@Thickness 1.60 mm
30.5 kV/in
@Thickness 0.0630 in
IEC 60243-1
Comparative Tracking Index 400 V400 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°FASTM C351
Thermal Conductivity 3.50 W/m-K24.3 BTU-in/hr-ft²-°Fthrough-plane, 10*10*3mm sample; ASTM E1461-07
 15.0 W/m-K104 BTU-in/hr-ft²-°Fin-plane, 25*0.4mm disc; ASTM E1461-07
Deflection Temperature at 0.46 MPa (66 psi) 275 °C527 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 275 °C
@Thickness 3.20 mm
527 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 242 °C
@Thickness 3.20 mm
468 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 130 °C266 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94  V-0
@Thickness >=1.00 mm
V-0
@Thickness >=0.0394 in
UL 94
 5VA
@Thickness >=2.50 mm
5VA
@Thickness >=0.0984 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 315 - 345 °C599 - 653 °F
Zone 3 315 - 345 °C599 - 653 °F
Melt Temperature 320 - 350 °C608 - 662 °FInjection Molding
Mold Temperature 110 - 150 °C230 - 302 °F
Drying Temperature 120 - 150 °C248 - 302 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 50 - 75 %50 - 75 %
Screw Speed 60 - 100 rpm60 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80643 / 288590

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.