MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: PTFE G Special Compound with steel

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.25 - 3.35 g/ccmolded; ASTM D792
Deformation 5.5 - 6.5 %
@Pressure 13.7 MPa,
Time 86400 sec
after 24hr relaxation; ASTM D621
 10 - 10.5 %
@Pressure 13.7 MPa,
Time 86400 sec
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 70molded; ASTM D2240
Tensile Strength 17.0 - 23.0 MPamolded; ASTM D4745
Elongation at Break 180 - 230 %molded; ASTM D4745
Compressive Yield Strength 10.0 - 10.5 MPa
@Strain 1 %
ASTM D695
Coefficient of Friction, Dynamic 0.13
K (wear) Factor 20.0 - 30.0 x 10-8 mm³/N-Mat PV 100; ASTM D3702
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 - 120 µm/m-°CASTM D696
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Overview of materials for Polyetheretherketone, PTFE Filled
Guarniflon PTFE G800 Polytetrafluoroethylene
Guarniflon PTFE G500 Polytetrafluoroethylene
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon

PGUARN014 / 142747

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.