MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer 4704 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with biocompatibility information and should not be used for medical applications which require biocompatibility. Alternative grade HPH4704.

Features: High Heat Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 1.20 g/ccASTM D792
Density 1.19 g/ccASTM D792
 1.20 g/ccISO 1183
Water Absorption 0.19 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.350 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.16 %ISO 62-1
Viscosity 2.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 2.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ASTM D785
Hardness, Rockwell R 127ASTM D785
Tensile Strength at Break 68.0 MPa50 mm/min; ISO 527
 77.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ASTM D638
 70.0 MPa50 mm/min; ISO 527
Elongation at Break 78 %50 mm/min; ASTM D638
 102 %50 mm/min; ISO 527
Elongation at Yield 7.0 %50 mm/min; ISO 527
 8.0 %50 mm/min; ASTM D638
Tensile Modulus 2080 MPa5 mm/min; ASTM D638
 2300 MPa1 mm/min; ISO 527
Flexural Strength 66.0 MPayield, 2 mm/min; ISO 178
 97.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2300 MPa2 mm/min; ISO 178
 2330 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 373 JASTM D256
 84.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 3204 J/mASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Tensile Impact Strength 577 kJ/m²ASTM D1822
Dart Drop, Total Energy 74.0 JASTM D3763
 149 JASTM D3029
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 2.50e+17 ohm-cmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
 3.27
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
Dissipation Factor 0.0016
@Frequency 50.0 - 60.0 Hz
ASTM D150
 0.026
@Frequency 100 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
 60 - 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
 15 - 30 arcs
@Thickness >=3.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 81.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Specific Heat Capacity 1.25 J/g-°CASTM C351
Thermal Conductivity 0.210 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 150 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 148 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 165 °CRate B/50; ISO 306
 167 °CRate B/120; ISO 306
 173 °CRate B/50; ASTM D1525
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.60ASTM D542
Haze 1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 85 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 365 °C
Zone 2 340 - 360 °C
Zone 3 350 - 370 °C
Melt Temperature 350 - 370 °CInjection Molding
Mold Temperature 80.0 - 115 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80071 / 288018

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.