MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akrochem Ribetak 7510 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: RUBETAK 7510 is an alkyl-phenol resin, thermoplastic type, in pastilles form.

Applications: RUBETAK 7510 is recommended as tackifier for synthetic and natural elastomers, featuring an excellent tack to green compounds make with synthetic or natural rubbers. This resin is specifically used in the manufacturing of tires, belts, hoses, etc.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.10 %<= 0.10 %
 
Chemical PropertiesMetricEnglishComments
Acid Value 50 - 7050 - 70[mg KOH/g], 739
 
Thermal PropertiesMetricEnglishComments
Melting Point 90.0 - 105 °C194 - 221 °FBall & Ring
 
Descriptive Properties
AppearanceAmber Pastilles
Content<0.3%Insoluble Acetone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH389 / 315307

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.