Product Description: Celanex 2003-5 is a general purpose, unreinforced polybuytlene terephthalate with a good balance of mechanical properties and processability for use in industrial and automotive applications. Celanex 2003-5 is a medium to high flow material that contains a small amount of an internal lubricant and nucleant. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Additive: Mold Release Use: Lighting Applications Forms: Pellets Processing Method: Injection Molding Information provided by Celanese |