MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Evonik X 50-S® Organosilane
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: X 50-S® is a blend of the bifunctional, sulfur-containing organosilane Si® 69 and N 330 type carbon black in the ratio 1:1 by weight. The product is applied in the rubber industry in combination with white fillers containing silanol groups.

Properties and applications: X 50-S® was developed for customers who prefer to handle Si 96® in a solid version. The Si 96® in the X 50-S® reacts with silanol groups of white fillers during mixing and with the polymer during vulcanization under formation of covalent chemical bonds. This imparts greater tensile strength, higher moduli, reduced compression set, increased abrasion resistance and optimized dynamic properties. X 50-S® is used in a variety of rubber products where silanol groups-containing white fillers are used and where optimum technical properties are required.

Application fields are: Low rolling resistance tires, Mechanical rubber goods, Shoe soles

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.770 g/cc0.0278 lb/in³Poured; ASTM D1513
Volatiles 2.0 %2.0 %ISO 787-2
Molecular Weight 532 g/mol532 g/mol
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 11.3 %11.3 %ASTM D6741
 
Descriptive Properties
Active substance0.5
Average sulfur chain length, HPLC3.7ASTM D6844

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIN022 / 317056

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.