MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Cabot CABELEC® CA6141 PC, Conductive Compound
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Conductive

Material Notes: Product highlights: CABELEC CA6141 electrically conductive compound is made from conductive carbon black dispersed in a modified polycarbonate and suitable for injection molding applications. It provides a good balance of electrical and mechanical properties that are not impacted by normal atmospheric conditions.

Key applications: CABELEC CA6141 conductive compound is used for packaging and electronic product handling applications where it is desirable to mitigate the hazard of electrostatic discharge. Examples of use are the handling and packaging of explosive powders, pigments and electronic components.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Linear Mold Shrinkage 0.070 - 0.090 cm/cm0.070 - 0.090 in/inASTM D955
Melt Flow  0.60 g/10 min
@Load 260 kg,
Temperature 2.16 °C
0.60 g/10 min
@Load 573 lb,
Temperature 35.9 °F
ISO 1133
 4.0 g/10 min
@Load 260 kg,
Temperature 5.00 °C
4.0 g/10 min
@Load 573 lb,
Temperature 41.0 °F
ISO 1133
 12 g/10 min
@Load 260 kg,
Temperature 10.0 °C
12 g/10 min
@Load 573 lb,
Temperature 50.0 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80
@Time 15.0 sec
80
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 47.0 MPa6820 psiISO 527
Tensile Strength, Yield 54.0 MPa7830 psiISO 527
Elongation at Break 24 %24 %ISO 527
Flexural Modulus 2.168 GPa314.4 ksiISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cmIEC 61340-2-3
Surface Resistance <= 1.00e+6 ohm<= 1.00e+6 ohmIEC 61340-2-3
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FISO 75/2
Vicat Softening Point 149 °C
@Load 1.02 kg
300 °F
@Load 2.25 lb
ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 °C518 °Fbarrel
Nozzle Temperature 290 °C554 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 120 °C248 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT047 / 315782

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.