MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Trigonox 125-CH75 tert-Amyl peroxypivalate, 75% solution in odorless mineral spirits
Categories: Other Engineering Material

Material Notes: Trigonox 125-CH75 is an (75% solution in odorless mineral spirits) initiator for (co)polymerization of styrene, ethylene, acrylonitrile, vinyl chloride, vinylidine chloride and (meth)acrylates, and polyols.

CAS number: 29240-17-3

EINECS/ELINCS No: 64741-65-7

Applications: Polymerization of ethylene: Trigonox 125-CH75 is an efficient initiator for the ethylene polymerization under high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, combinations with other peroxides are applied in practice. Polymerization of vinyl chloride: Trigonox 125-CH75 can be applied as an initiator for the suspension polymerization of vinyl chloride in the temperature range between 50°C and 65°C. Trigonox 125-CH75 may be used in combination with other initiators to increase reactor efficiency.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.888 g/cc
@Temperature -10.0 °C
0.0321 lb/in³
@Temperature 14.0 °F
Half-life  0.100
@Temperature 91.0 °C
0.100
@Temperature 196 °F
[hr]
 1.00
@Temperature 72.0 °C
1.00
@Temperature 162 °F
[hr]
 10.0
@Temperature 54.0 °C
10.0
@Temperature 129 °F
[hr]
Viscosity 4.0 cP
@Temperature -10.0 °C
4.0 cP
@Temperature 14.0 °F
Molecular Weight 188.3 g/mol188.3 g/mol
Storage Temperature -30.0 - -10.0 °C-22.0 - 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 25.0 °C77.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay74.0-76.0 %
Color= 20 Pt-Co / APHA
Content= 0.1 %Hydroperoxides as TAHP
 = 150 mg/kgInorganic + organic hydrolysable chloride
 6.29-6.46 %Active oxygen
Content (%)8.5Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1004 / 286527

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.