MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Daplen™ ED113AE Polypropylene, 15% Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen™ ED113AE is a 15% mineral filled polypropylene compound intended for injection molding. This material provides excellent paintability, very good impact/stiffness balance and it is easy to process.

Special Features:

  • Very good processability
  • High level of surface aspects, meeting the more stringent paint adhesion requirements
  • Low density with good impact/stiffness balance enabling weight reduction
  • Primerless paintable allowing optimization of painting cycle time and reduction of system costs
  • Low thermal expansion over a broad temperature scale for zero-gap applications
Applications: Daplen ED113AE has been developed especially for the automotive industry and is suitable for applications like:
  • Bumpers
  • Automotive exterior applications
  • Rocker panels
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO 1183
Melt Flow 8.50 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.50 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.0 MPa2470 psiISO 527-2
Tensile Modulus 1.70 GPa247 ksiISO 527-2
Charpy Impact, Notched  0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 3.50 J/cm²
@Temperature 23.0 °C
16.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 66.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
36.7 µin/in-°F
@Temperature -22.0 - 176 °F
Deflection Temperature at 0.46 MPa (66 psi) 102 °C216 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Feed Temperature 40.0 - 80.0 °C104 - 176 °F
 220 - 260 °C428 - 500 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
 
Descriptive Properties
Flow front speed100 - 200 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9683 / 323040

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.