Description: BRALEN+ FB 08-12 is a film grade of low density polyethylene. This grade is additives free. Applications: BRALEN+ FB 08-12 is suitable for production of non-slip shrink films for collation packaging, technical films, bags and pouches. This grade can be used also for blow molding applications. Recommended film thickness is 0.025 to 0.100 mm. (1) Density has been measured on pressed mould specimen according to internal method. (2) Film properties tested using 50 µm thick blown film extruded at melt temperature of 180 °C and blow up ratio 2.5:1. (3) Typical properties measured on standard injection molded test specimen according to ISO 294-1. Information provided by Molgroup Chemicals |