MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Michelman® Michem® Coat 81 Water resistant coating with intermediate moisture barrier.
Categories: Fluid; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Michem® Coat water-based coatings are selected primarily for grease and oil resistance. Other benefits include water resistance, release, coldset gluability, hot melt gluability, recyclability, and compliance with specific food contact regulations. Michem® Coat 81 is best applied via off-line rod coater or in-line at the wet end of the corrugator. Dry end application is not recommended. Dilution is not recommended. Usage: A repulpable, printable, and cold set gluable coating optimized for water resistance and intermediate MVTR protection. Common uses include packaging for produce and meats, or anywhere packaged goods require protection from water or moisture vapor. It can be used alone as a single bump, or can be an ideal base coat for other barrier-enhancing Michelman coatings.

Applications (properties imparted): Industrial (skid resistance), Perishables (water resistance).

Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required.

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 8.5 - 108.5 - 10
Brookfield Viscosity 400 - 800 cP400 - 800 cPSpindle #3. 60 RPM.
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 MonthDry, cool and well-ventilated place
 
Descriptive Properties
AppearanceOff-white liquid
Solids TypePolymer / Pigment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WMICHE9894 / 287489

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.