MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin GFN30F Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ GFN30F resin is a 30% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN30F carries a UL746C outdoor suitability rating of F2 along with FDA food contact compliance and NSF 61 listings in several colors. The properties of this material makes it an excellent candidate for water management applications such as water filter and meter components, pump housings / impellers, shower + faucet, and valves.*See NORYL GFN30 resin for NON FDA / NSF version.

Features: Hydrolytic Stability,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.0400 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.10 %ISO 62-1
Viscosity 2.0 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 3.2 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa50 mm/min; ISO 527
 130 MPa50 mm/min; ASTM D638
Elongation at Break 2.5 %50 mm/min; ISO 527
 3.0 %50 mm/min; ASTM D638
Tensile Modulus 8200 MPa1 mm/min; ISO 527
 8600 MPa5 mm/min; ASTM D638
Flexural Strength 160 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 160 MPayield, 2 mm/min; ISO 178
Flexural Modulus 6800 MPa2 mm/min; ISO 178
 7200 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 100 JASTM D256
 120 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 590 J/mASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
Charpy Impact, Notched 8.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 20.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 23.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 139 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 139 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 147 °CRate B/50; ASTM D1525
 147 °CRate B/50; ISO 306
 149 °CRate B/120; ISO 306
UL RTI, Electrical 90.0 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 90.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 300 - 325 °C
Zone 2 275 - 320 °C
Zone 3 290 - 325 °C
Melt Temperature 300 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF2UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82325 / 290272

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.