MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SPERSE® PG 001 Aqueous Dispersions
Categories: Other Engineering Material

Material Notes: Product Highlights: CAB-O-SPERSE PG 001 aqueous silica dispersion is well suited for use in microporous coatings formulations for inkjet media and is characterized by:
  • Low viscosity
  • High solids loading
  • Median particle diameter less than 0.2 microns
Key Applications
Inkjet Media: CAB-O-SPERSE PG 001 aqueous silica dispersion can be used in microporous coatings for inkjet printing. Microporous coatings enable instant dry printing, a significant improvement over slow drying polymer swellable coatings. The product’s high adsorptive capacity enables fast adsorption of inks and rapid drying speed.

Performance Features:

  • Enables faster drying time
  • Porosity
  • Well-suited for semi-gloss (satin) photo paper

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormAqueous dispersion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT113 / 315848

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.