Product Description: Mansil 065 is a white, spray-dried, precipitated silica. It is a semi-reinforcing filler for use in synthetic and natural rubber compounding. The spray-dried silicas have a larger particle size than the milled type silicas. Advantages are faster incorporation time and less viscosity buildup while maintaining excellent dispersion. Applications: Precipitated silica increases hardness, tensile strength, abrasion and tear resistance. For mechanical rubber goods, Mansil-065 can be used as the primary filler or in combination with carbon black. In tire applications, these silicas improve rolling resistance, flex fatigue and enhance traction. In adhesives compounding, silica provides an additional method of promoting improved adhesion, as well as providing reinforcement. Silicas are universally applied to provide increased abrasion resistance, green strength and translucence in the formulating of shoe sole compounds. Information provided by Akrochem Corporation |