MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
M. Holland Company GS411 Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good Flow

Uses: Disposable Drinkware, Electrical/Electronic Applications

Approvals: FDA 21 CFR 177.1640

Processing Method: Extrusion, Injection Molding

Information provided by M. Holland.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Melt Flow 11 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5500 psiASTM D638
Elongation at Break 1.5 %ASTM D638
Tensile Modulus 445000 psiASTM D638
Flexural Strength 11000 psiASTM D790
Flexural Modulus 500000 psiASTM D790
Izod Impact, Notched 0.350 ft-lb/in0.125 in; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 197 °FUnannealed; ASTM D648
Vicat Softening Point 210 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet)
Lucite International Colacryl® P2601 Specialty Polystyrene Resin
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
I. Stern N2560 General Purpose Crystal Polystyrene
Cyclewood Solutions Xylomer™ XM2-CUA Sustainable Injection Molding Resin

PMH017 / 52950

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.