Vydyne 21SPR is a general-purpose, unfilled, PA66 resin with an performance lubricant. Designed principally for injection-molding applications, this product offers a combination of engineering properties characterized by high strength; rigidity; good toughness; high melt point; good surface lubricity; abrasion resistance; and resistance to many chemicals, machine and motor oils, solvents and gasoline.Information provided by Ascend Performance Materials. |