MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-FRPC Flame Retardant for PC
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP) has developed a flame retardant that is especially for PC industry - GY-FR-PC which is a non-halogen flame retardant that provides outstanding flame retardant effect. It is with high thermal stability and compatible with various PC products. GY-FR-PC can also improve the processibility and heat resistance of PC and resins.

Intro: PC are a group of thermoplastic polymers with good properties that find many applications. The needs for PC are gradually growing in construction industry, automobile industry, electronics industry, and so forth. However, PC is combustible; as a result, the needs for flame retardant for this material are becoming popular. GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP) has developed a flame retardant that is especially for PC industry - GY-FR-PC which is a non-halogen flame retardant that provides outstanding flame retardant effect. It is with high thermal stability and compatible with various PC products. GY-FR-PC can also improve the processibility and heat resistance of PC and resins.

Advantages:

  • Non-halogen flame retardant
  • Provides excellent flame-retardant effect and impact resistance to the product
  • With great thermal stability
  • Improves the processibility and heat resistance of PC and resins
  • Increases the value of a product
Applications:
  • Any kinds of PC products
  • Outer skin of vehicles and scooters
  • Automotive parts
  • PC signboard, construction board
  • Smartphone case, computer case, TV shell
  • Lampshade, light tube, lens, bullet-proof glass
  • Sport bottle, milk bottle

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 6.5 - 7.5
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.8 %
 
Descriptive Properties
AppearancePowder
ColorWhite
Composition? 0.5%DPS
 <5 ppmIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN036 / 266344

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.