MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyram PA700 Nylon 6.6, UV Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: UV stabilized polyamide 6.6 for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDIN 53479
Water Absorption 8.5 %DIN 53495
Moisture Absorption at Equilibrium 2.8 %50%RH; DIN 53714
Linear Mold Shrinkage 0.011 - 0.018 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM-D785
Tensile Strength, Yield 85.0 MPaASTM-D638
Elongation at Break 40 %ASTM-D638
Flexural Strength 115 MPaASTM D790
Flexural Modulus 2.60 GPaASTM-D790
Izod Impact, Notched 0.600 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmDIN 53482
Surface Resistance 1.00e+13 ohmDIN 53482
Dielectric Constant 3.3
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 120 kV/mmVDE 0303/4
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °C
Maximum Service Temperature, Air 110 °CContinuous Use
 >= 180 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 235 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °CDIN 53461
Flammability, UL94 V-2
@Thickness 3.00 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® B3 GF 20 2 RM-D (3375) PA 6 Dry, 20% Glass Fiber Filled
Akro-Plastic Akromid® B3 GF 30 2 RM-D black (3424) PA 6 + ABS Dry, 30% Glass Filled
Celanese Zytel® 74G33W BK196 PA66+PA6-GF33
Polyram PlusTek PB702 Nylon 6, UV Stabilized
Polyram PlusTek RA844 Nylon 6.6, UV Stabilized

PPOLYRA248 / 57510

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.