SABIC LNP™ THERMOCOMP™ Compound DF004P Polycarbonate (PC) (Americas)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LNP THERMOCOMP DF004P compound is based on Polycarbonate (PC) resin containing 20% glass fiber. Added features of this grade include: Exceptional Processing.
Features: High Stiffness,Exceptional Processing,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.34
g/cc
1.34
g/cc
ASTM D792
Moisture Absorption
0.0200 %
0.0200 %
Injection Molding
0.120 %
0.120 %
23°C/50% RH/24 hrs; ASTM D570
0.190 %
0.190 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0020
cm/cm
0.0020
in/in
24hrs; ASTM D955
0.0023
cm/cm
0.0023
in/in
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.0067
cm/cm
0.0067
in/in
24hrs; ISO 294
0.0070
cm/cm
0.0070
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
102
MPa
14800
psi
ISO 527
104
MPa
15100
psi
ASTM D638
Elongation at Break
3.2 %
3.2 %
ASTM D638
3.2 %
3.2 %
ISO 527
Tensile Modulus
6.19
GPa
898
ksi
5 mm/min; ASTM D638
6.20
GPa
899
ksi
1 mm/min; ISO 527
Flexural Strength
162
MPa
23500
psi
ISO 178
172
MPa
24900
psi
ASTM D790
Flexural Modulus
5.99
GPa
869
ksi
ISO 178
6.17
GPa
895
ksi
ASTM D790
Izod Impact Notched
74.0
J
54.6
ft-lb
ASTM D256
Izod Impact, Unnotched
7.25
J/cm
13.6
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
9.00
kJ/m²
4.28
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
47.0
kJ/m²
22.4
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
8.00
J
5.90
ft-lb
peak; ASTM D3763
Impact Test
2.00
J
1.48
ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
33.4
µm/m-°C
@Temperature -40.0 - 40.0 °C
18.6
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
33.5
µm/m-°C
@Temperature -40.0 - 40.0 °C
18.6
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow
54.5
µm/m-°C
@Temperature -40.0 - 40.0 °C
30.3
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
68.9
µm/m-°C
@Temperature -40.0 - 40.0 °C
38.3
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)
139
°C
282
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
138
°C
@Thickness 3.20 mm
280
°F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical
80.0
°C
176
°F
UL 746B
UL RTI, Mechanical with Impact
80.0
°C
176
°F
UL 746B
UL RTI, Mechanical without Impact
80.0
°C
176
°F
UL 746B
Flammability, UL94
V-2
@Thickness >=1.50 mm
V-2
@Thickness >=0.0591 in
UL 94
V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
Processing Properties
Metric
English
Comments
Zone 2
310
-
320
°C
590
-
608
°F
Zone 3
320
-
330
°C
608
-
626
°F
Melt Temperature
305
-
325
°C
581
-
617
°F
Injection Molding
Mold Temperature
80.0
-
110
°C
176
-
230
°F
Drying Temperature
120
°C
248
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81520 / 289467
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.