Description: - PA1003 is a nylon-based dielectric absorber.
- Designed for attenuation in the +10 GHz range.
- This product line is designed to make rigid parts requiring mechanical properties.
- PA1003 has been impact modified to provide toughness and impact resistance.
- Ideally suited to be molded into a connector, housing, or circuit cover.
- Performance can be tailored to specific applications.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |