MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ ELCRIN™ WF0061iQ Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP ELCRIN WF0061iQ compound is based on Polybutylene terephthalate (PBT) resin utilizing ELCRIN iQ upcycling technology containing minimum 25% Post-Consumer Recycling (PCR) weight content and 30% glass fiber. Added features of this grade include: Non-Chlorinated, Non-Brominated Flame Retardant, UL94V0 and 5VA Flame Rating, Excellent Chemical Resistance. This is a good candidate for a variety of applications needing a more sustainable FR and PBT solution.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Enhanced Chemical Resistance,Flame Retardant,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.56 g/cc1.56 g/ccASTM D792
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0900 %0.0900 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %0.23 %ISO 62-1
Viscosity 16 cP
@Load 5.00 kg,
Temperature 250 °C
16 cP
@Load 11.0 lb,
Temperature 482 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0028 cm/cm
@Thickness 3.20 mm
0.0028 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0057 cm/cm
@Thickness 3.20 mm
0.0057 in/in
@Thickness 0.126 in
SABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psi5 mm/min; ASTM D638
 108 MPa15700 psi5 mm/min; ISO 527
Tensile Strength, Yield 105 MPa15200 psi5 mm/min; ASTM D638
 108 MPa15700 psi5 mm/min; ISO 527
Elongation at Break 2.0 %2.0 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %2.0 %5 mm/min; ASTM D638
 2.0 %2.0 %5 mm/min; ISO 527
Tensile Modulus 11.0 GPa1600 ksi5 mm/min; ASTM D638
 11.0 GPa1600 ksi1 mm/min; ISO 527
Flexural Strength 165 MPa23900 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 165 MPa23900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 175 MPa25400 psibreak, 2mm/min; ISO 178
 175 MPa25400 psiyield, 2 mm/min; ISO 178
Flexural Modulus 9.60 GPa1390 ksi1.3 mm/min, 50 mm span; ASTM D790
 10.0 GPa1450 ksi2 mm/min; ISO 178
Izod Impact Notched 72.0 J53.1 ft-lbASTM D256
 55.0 J
@Temperature -30.0 °C
40.6 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 5.70 J/cm10.7 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²3.33 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 37.0 kJ/m²17.6 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J4.43 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VIEC 60112
Hot Wire Ignition, HWI  60 - 120 sec
@Thickness >=0.800 mm
60 - 120 sec
@Thickness >=0.0315 in
UL 746A
 >= 120 sec
@Thickness >=3.00 mm
>= 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.800 mm
>= 120 arcs
@Thickness >=0.0315 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 24.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
13.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 214 °C
@Thickness 3.20 mm
417 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
@Thickness 3.20 mm
392 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 75.0 °C167 °FUL 746B
UL RTI, Mechanical with Impact 75.0 °C167 °FUL 746B
UL RTI, Mechanical without Impact 75.0 °C167 °FUL 746B
Flammability, UL94  V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL 94
 5VB
@Thickness >=3.00 mm
5VB
@Thickness >=0.118 in
UL 94
Glow Wire Ignition Temperature  750 °C
@Thickness 0.800 mm
1380 °F
@Thickness 0.0315 in
IEC 60695-2-13
 775 °C
@Thickness 1.50 mm
1430 °F
@Thickness 0.0591 in
IEC 60695-2-13
 800 °C
@Thickness 3.00 mm
1470 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 230 - 255 °C446 - 491 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 240 - 260 °C464 - 500 °F
Melt Temperature 245 - 260 °C473 - 500 °FInjection Molding
Mold Temperature 40.0 - 100 °C104 - 212 °F
Drying Temperature 110 - 120 °C230 - 248 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Precipitation Temperature 40.0 - 60.0 °C104 - 140 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80616 / 288563

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.