MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC PC0703 PC (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC0703 resin is a low flow (MFR = 7 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product designed for use in the extrusion market.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Density 1.20 g/ccISO 1183
Moisture Absorption at Equilibrium 0.35 %ASTM D570
Water Absorption at Saturation 0.35 %ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmon Tensile Bar; SABIC Method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Melt Index of Compound 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
MVR [cm^3/10 min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
 120ISO 2039-2
Tensile Strength, Yield 63.0 MPaType I, 50 mm/min; ASTM D638
 63.0 MPa50 mm/min; ISO 527
Elongation at Break >= 70 %Type I, 50 mm/min; ASTM D638
 >= 70 %50 mm/min; ISO 527
Elongation at Yield 6.0 %Type I, 50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2350 MPa50 mm/min; ASTM D638
 2350 MPa1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 90.0 MPa2 mm/min; ISO 178
Flexural Modulus 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
 2300 MPa2 mm/min; ISO 178
Izod Impact, Notched 900 J/mASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Dart Drop, Total Energy 65.0 JInstrumented Impact Energy @ peak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
 >= 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
 3.0
@Frequency 60 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 27.0 kV/mm
@Thickness 1.60 mm
ASTM D149
 27.0 kV/mm
@Thickness 1.60 mm
IEC 60243-1
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
 0.0010
@Frequency 60 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E 831
 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KASTM C177
 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 138 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 138 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
ASTM D648
Vicat Softening Point 144 °CRate B/50; ASTM D1525
 144 °CRate B/50; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm
UL 94
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
 1.586ISO 489
Haze <= 0.80 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 88 - 90 %2.54 mm; ASTM D1003
 
Descriptive Properties
Ball Pressure Test, 125°C +/- 2°CPassesIEC 60695-10-2

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI54343 / 154389

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.