  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Impet® HD250 PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Product Description: A highly filled PET which has an excellent balance of mechanical properties, processability and high density. Impet HD250 is specifically designed to exhibit a ceramic-like feel.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Impact Modifier

Features: Impact Modified

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.50 g/ccISO 1183
Maximum Moisture Content 0.010
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6090 psiISO 527-2/5
Elongation at Break 1.1 %ISO 527-2/5
Flexural Strength 10500 psiISO 178
Flexural Modulus 1.12e+6 psiISO 178
Charpy Impact, Notched 1.70 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 1.90 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistance 300 ohmIEC 62631-3-2
Arc Resistance >= 124 sec
Comparative Tracking Index >= 600 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 468 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 394 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 491 - 509 °F
Middle Barrel Temperature 491 - 509 °F
Front Barrel Temperature 500 - 529 °F
Zone 4 509 - 540 °FInjection
Melt Temperature 520 - 559 °F
Mold Temperature 248 °F
Drying Temperature 275 °F
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6294 / 310987

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.