MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc 70-3812 NC High Thermal Transfer Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 70-3812 NC is a two component, aluminum filled epoxy system. This system is used for making heat resistant tools, parts, or bonds that require the highest thermal conductivity and heat resistance. We have developed this extremely conductive epoxy by formulating it with a unique combination of fillers, particle sizes and dispersion techniques. 70-3812 NC has good heat dissipation making this a popular choice for a variety of heat sink applications. Common heat sink bonding applications include fin to base, folded-fin set to base, pin-fin set to base, and cold plate tube to extruded base. The 70-3812RNC is formulated with high performance materials and additives that give heat sink manufacturers improved adhesion and processing advantages. 70-3812 NC passes NASA’s outgassing requirements per ASTM E-595-07.

Features:

  • Excellent Thermal Conductivity
  • Superior Adhesion
  • Low Viscosity allows quick self leveling Information provided by Epoxies, Etc
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/cc
Viscosity 8000 cPMixed
 130000 cPResin
Outgassing - Total Mass Loss 0.070 %CVCM
 0.91 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65
@Temperature 100 °C
 90
@Temperature 25.0 °C
Tensile Strength 2500 psiAluminum to Aluminum 1” overlap
Compressive Strength 18500 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°C
Thermal Conductivity 4.50 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 - 20.0 min
@Temperature 125 °C
 24.0 hour
@Temperature 25.0 °C
 45.0 min
@Temperature 65.0 °C
 
Descriptive Properties
ColorGrey
Mix Ratio100:10by weight
Working Time100 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX063 / 316740

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.